Blue Parlon
Amount Wanted
Total:
Summary
Bind with acetone, add 5 Ti for tail [after screening]. Copper Oxide can be substituted 1:1 for the Copper Carbonate with good results. Optimized for screen extrusion technique
Bind with acetone, add 5 Ti for tail [after screening]. Copper Oxide can be substituted 1:1 for the Copper Carbonate with good results. Optimized for screen extrusion technique